The invention consists in mixing clay, sand, a calcium-containing reactant, an alkali metal hydroxide and water, in forming this mixture, for example by extrusion, drying and maturing as far as the shrinkage limit and finally in heating in two stages at atmospheric pressure, the first in moist atmosphere at a temperature between 95 and 105 DEG C, and the second at a temperature of the order of ...